Thermal Break Assembly Machine(Three Steps):
Function: make thermal break aluminum profile
Raw material: PA66 thermal break strip
Including: knurling machine, strip feeding machine, crimping machine, testing machine
Process:
1,knurling tooth in slot of profile, increase shear strength
2,insert thermal break strip in slot of profile where has been knurled
3,rolling aluminum profile to combine strip with profile tightly
4, test shear strength is good or not
Parameters:
Knurling machine:
Total power of motor |
1.1KW (0.55KW×2) |
Knurling adjustable size |
height:0~260mm; width:0~260mm |
Diameter of knurling blade |
φ80 |
Overall dimension |
1040mm×1350mm×1550mm |
Compressed air |
0.6~1.0Mpa |
speed |
0~70m/min |
Profile size |
260mm×200mm |
weight |
约1000kg |
Strip feeding machine:
Diameter of feeding roller |
Φ160 |
Speed of feeding profile |
0~70m/min |
Feeding adjustable size |
0~150 mm |
Single side adjustable height |
0~100 mm |
Height of strip |
12~40 mm |
Compressed air |
0.6~1.0Mpa |
Total power of motor |
1.1KW |
weight |
About 1000kg |
Overall dimension |
L 1000 mm×W 650 mm×H 1300 mm |
Rolling combining machine:
Profile size |
260mm×380 mm |
Steel roller diameter |
φ238 |
Total power |
Power of main motor:3KW Power of lifting motor:0.55KW |
Overall dimension |
1220mm×1300mm×1350mm |
speed |
0~70m/min |
Roller adjustable height |
width:0~100mm |
weight |
About 1800kg |
Thermal Break Assembly Machine(Three Steps)
Make thermal break aluminum profile,PA66 thermal break strip